ASTM A453 Grade 660 is bolting made from A286, an age-hardened iron-nickel-chromium alloy (UNS S66286), for high-temperature service. It is used on turbines, exhaust systems and hot process equipment. The grade comes in four classes, A, B, C and D, which differ in heat treatment and strength.

A453 Grade 660 bolting from Eastwood

  • A286 studs, bolts and cap screws to A453 Grade 660, in the class on your drawing
  • A286 hex nuts on our stock shelf, aged and passivated, from domestic DFARS-compliant material
  • Stainless and A286 parts passivated in house
  • Material certifications with heat numbers shipped with the order
  • PPAP documentation at Levels 1 to 5, for a fee
  • An AS9100D and ISO 9001:2015 certified shop in Houston, Texas
Request a quote

Classes

All four classes use the same alloy. The class sets the solution treatment and aging, and that sets the strength. Classes A, B and C have the same minimum strength; Class D has a higher yield strength and is not stress-rupture tested.

Strength

ClassTensile, min (ksi)Yield, min (ksi)Elongation, min (%)Reduction of area, min (%)Hardness
A, B, C130851518248 to 341 HBW, 24 to 37 HRC
D, 2-1/2 in. and under1301051518248 to 321 HBW, 24 to 35 HRC
D, over 2-1/2 in.120951518248 to 321 HBW, 24 to 35 HRC
Class A, B, CTensile: 130 ksiTensile 130Yield: 85 ksiYield 85Class D, to 2-1/2 in.Tensile: 130 ksiTensile 130Yield: 105 ksiYield 105Class D, over 2-1/2 in.Tensile: 120 ksiTensile 120Yield: 95 ksiYield 95
Class D trades the stress-rupture test for a higher yield strength. Tensile and yield minimums in ksi.

Heat treatment

ClassSolution treatmentAging (hardening)
A1650°F, 2 h minimum, liquid quench1325°F, 16 h, air cool
B1800°F, 1 h minimum, liquid quench1325°F, 16 h, air cool
C1800°F, 1 h minimum, oil quench1425°F, 16 h, air cool, then 1200°F, 16 h, air cool
DAs Class A or Class B1325°F, 16 h, air cool; optional second age at 1200°F, 16 h

All temperatures are plus or minus 25°F. State the class on the drawing or the request, because the class fixes the heat treatment.

Stress rupture

ClassesTest temperatureStressMinimum time to ruptureMinimum elongation
A, B, C1200°F (650°C)56 ksi100 h5%
DNot required

Chemistry

ElementPercent
Nickel24.0 to 27.0
Chromium13.5 to 16.0
Titanium1.90 to 2.35
Molybdenum1.00 to 1.50
Vanadium0.10 to 0.50
Boron0.001 to 0.010
Manganese, max2.00
Silicon, max1.00
Aluminum, max0.35
Carbon, max0.08
Phosphorus, max0.040
Sulfur, max0.030
IronBalance

Thread types

TypeHow the threads are made
M1Machined after aging
M2Machined after solution treatment, before aging
R1Rolled after aging
R2Rolled after solution treatment, before aging

If the drawing gives a thread type, we make it that way. If it does not, we ask before we cut.

Grade marks

Parts are marked with the grade and class, such as 660A, with the thread type and the manufacturer's mark.

660A660B660C660D
The grade and class symbol on the end of the stud.

Common questions

What is ASTM A453 Grade 660?

A453 Grade 660 is bolting made from A286 alloy (UNS S66286) for high-temperature service. It comes in Classes A, B, C and D, which differ in heat treatment and strength.

Is A453 Grade 660 the same as A286?

Grade 660 is made from A286 alloy. A453 adds the heat treatment, strength, testing and marking requirements for bolting.

What is the difference between Class A, B, C and D?

A, B and C use different solution and aging treatments but share 130 ksi tensile and 85 ksi yield minimums and a stress-rupture test. Class D has 105 ksi yield up to 2-1/2 in. and no stress-rupture test.

What do M1, M2, R1 and R2 mean?

They describe how the threads are made: machined (M) or rolled (R), after aging (1) or after solution treatment and before aging (2).

Does Eastwood stock A286 nuts?

Yes. A286 hex nuts are on our stock shelf, aged and passivated, from domestic DFARS-compliant material. Studs and bolts are made to order.

What is ASTM A453 grade 660 material used for?

High temperature bolting where alloy steels lose strength: gas and steam turbines, aircraft engines and high temperature process equipment. Grade 660 is the ASTM bolting name for A286 superalloy.

Sizes Eastwood makes

We machine studs from bar up to 3.000 in. diameter, with small diameters on our Swiss machines. Hex bolts and cap screws are smaller, because the head sets the bar size. Larger parts are quoted too.

A286 alloy fasteners · Inconel 718 fasteners · ASTM A193 · Aerospace · Power generation · Quality, certifications and PPAP

Quote A453 Grade 660 parts

Send the class, thread type, diameter, length and quantity, or send the print. Add any coating, testing, PPAP or sour-service requirement and the date you need the parts. Lead time comes back with the price.

Request a quote sales@emfasteners.com

The tables summarize requirements from ASTM A453/A453M. The standard itself governs. Check the current edition for your order.