ASTM A194 Heavy Hex Nuts
ASTM A194 covers carbon steel, alloy steel and stainless steel nuts for high-pressure or high-temperature service. The common grades are 2H, 2HM, 7, 7M, 8 and 8M, and they are the nuts that go on A193 and A320 studs.
A194 nuts from Eastwood
- Heavy hex and hex nuts to A194, matched to the studs on the same order
- Heat treatment done in house or by outside heat treaters, to the grade's requirements
- Material certifications with heat numbers shipped with the order
- PPAP documentation at Levels 1 to 5, for a fee
- An AS9100D and ISO 9001:2015 certified shop in Houston, Texas
- Stainless grades passivated in house
Grades
| Grade | Material | Condition |
|---|---|---|
| 2H | Carbon steel | Quenched and tempered |
| 2HM | Carbon steel | Quenched and tempered to a lower hardness; every nut tested |
| 7 | Alloy steel (4140 type) | Quenched and tempered |
| 7M | Alloy steel | Quenched and tempered to a lower hardness; every nut tested |
| 8 | 304 stainless | As specified for the class |
| 8M | 316 stainless | As specified for the class |
Grade 4 nuts were withdrawn from A194 in 2017. Drawings that still call out Grade 4 are usually supplied with Grade 7.
Hardness and proof stress
| Grade | Hardness of finished nut | Proof stress, heavy hex (ksi) | Minimum tempering |
|---|---|---|---|
| 2H, to 1-1/2 in. | 248 to 327 HBW, 24 to 35 HRC | 175 | 850°F |
| 2H, over 1-1/2 in. | 212 to 327 HBW, 35 HRC max | 175 | 850°F |
| 2HM | 159 to 235 HBW, 84 to 99 HRB | 150 | 1150°F |
| 7 | 248 to 327 HBW, 24 to 35 HRC | 175 | 1100°F |
| 7M | 159 to 235 HBW, 84 to 99 HRB | 150 | 1150°F |
| 8, 8M | 126 to 300 HBW | 80 | None |
Proof stress is the stress the nut must carry on a hardened mandrel without stripping or cracking. Plain hex nuts, as opposed to heavy hex, have lower proof stress values in the standard.
Chemistry
| Element (%) | 2H, 2HM | 7, 7M | 8 (304) | 8M (316) |
|---|---|---|---|---|
| Carbon | 0.40 min | 0.38 to 0.48 | 0.08 max | 0.08 max |
| Manganese | 1.00 max | 0.75 to 1.00 | 2.00 max | 2.00 max |
| Phosphorus, max | 0.040 | 0.035 | 0.045 | 0.045 |
| Sulfur, max | 0.050 | 0.040 | 0.030 | 0.030 |
| Silicon | 0.40 max | 0.15 to 0.35 | 1.00 max | 1.00 max |
| Chromium | 0.80 to 1.10 | 18.0 to 20.0 | 16.0 to 18.0 | |
| Nickel | 8.0 to 11.0 | 10.0 to 14.0 | ||
| Molybdenum | 0.15 to 0.25 | 2.00 to 3.00 |
The Grade 7 ranges are current-edition heat analysis limits. Older editions printed slightly wider ranges, such as carbon 0.37 to 0.49.
Which stud each nut matches
| Stud | Usual A194 nut |
|---|---|
| A193 B7 | 2H |
| A193 B7M | 2HM |
| A193 B16 | 7 |
| A193 B8, Class 1 or 2 | 8 |
| A193 B8M, Class 1 or 2 | 8M |
| A320 L7 and L43 | 7 |
| A320 L7M | 7M |
Order nuts and studs together when you can, so the certifications for the set arrive as one package. See ASTM A193 and ASTM A320 for the studs.
Grade marks
A194 nuts carry the grade symbol and the manufacturer's mark on one face. M grades are marked with the M, so a 2HM nut can be told from a 2H nut in the field.
The M grades
2HM and 7M are held to 235 HBW maximum and every nut is hardness tested, not a sample from the lot. They are the nuts for sour service, where hydrogen sulfide is present, and they pair with B7M and L7M studs. A 2H nut on a B7M stud defeats the point of the B7M. If your specification cites NACE MR0175 / ISO 15156 or NACE MR0103, put it on the request.
2H or 7
Both are rated at 175 ksi proof stress on a heavy hex nut. 2H is carbon steel and is the standard nut for B7 studs. Grade 7 is alloy steel, tempered at a higher temperature, and is the usual nut for B16 studs and for A320 low-temperature studs. If the drawing calls for 2H, we quote 2H.
A194 or A563
| A194 | A563 | |
|---|---|---|
| Service | High pressure or high temperature | General structural and mechanical |
| Typical grade | 2H heavy hex | DH heavy hex |
| Goes on | A193 and A320 studs | A307, A449, F3125 A325 and A490 bolts |
| Substitution | 2H may replace A563 DH on Type 1 structural bolts | Not a substitute in A194 service |
Common questions
What is an A194 2H nut?
A heavy hex nut made of carbon steel, quenched and tempered, with a proof stress of 175 ksi. It is the standard nut for A193 B7 studs.
What is the difference between 2H and 2HM?
2HM is tempered to a lower hardness, 235 HBW maximum, and every nut is hardness tested. It is used in sour service with B7M studs. 2H is harder and stronger.
Can an A194 2H nut be used instead of an A563 DH nut?
A194 2H heavy hex nuts are commonly accepted in place of A563 DH. Check your project specification before substituting.
Which A194 nut goes with a B7 stud?
Grade 2H. B7M takes 2HM, B16 takes Grade 7, B8 takes Grade 8 and B8M takes Grade 8M.
What happened to A194 Grade 4?
Grade 4 was withdrawn from A194 in 2017. Grade 7 is the usual replacement.
What is ASTM A194 material?
It depends on the grade. 2H and 2HM are carbon steel, quenched and tempered. Grade 7 is alloy steel. 8 and 8M are 304 and 316 stainless steel.
Is ASTM A194 grade 2H stainless steel?
No. 2H is quenched and tempered medium carbon steel. The stainless A194 grades are 8 (304) and 8M (316).
What is the main difference between ASTM A193 and A194?
A193 covers the studs and bolts; A194 covers the nuts that go on them. A B7 stud normally takes an A194 2H heavy hex nut.
Sizes Eastwood makes
We machine studs from bar up to 3.000 in. diameter, with small diameters on our Swiss machines. Hex bolts, cap screws and nuts are smaller, because the hex sets the bar size. Larger parts are quoted too.
Related pages
ASTM A193 · A193 Grade B7 studs · ASTM A320 · Specialty nuts · Oil and gas · Quality, certifications and PPAP
Industries that use this spec: Oil and Gas · Chemical Refining · Power Generation
Other specification guides: ASTM F1554 anchor rods · ASTM A325 structural bolts · ASTM A193 · A193 Grade B7 · ASTM A320 · ASTM A453 Grade 660 · ASTM A354 · ASTM F593 and F594 · SAE J429 Grades 5 and 8 · ASTM A574 socket head cap screws · ASTM A307 · ASTM A449 · ASTM A563 nuts · ASTM F436 washers · ASTM A490 structural bolts
Quote A194 nuts
Send the grade, thread size, heavy hex or hex, quantity and the studs they go with, or send the print. Add any coating, testing, PPAP or sour-service requirement and the date you need the parts. Lead time comes back with the price.
Request a quote sales@emfasteners.com
The tables summarize requirements from ASTM A194/A194M. The standard itself governs. Check the current edition for your order.